AMACO Kiln Ice (KI) Series
AMACO Brent presents the Kiln Ice (KI) Series, a new collection of six mid-range (Cone 5–6) crystalline-inspired glazes released in the summer of 2025. These glazes are designed to capture the quiet beauty of frozen surfaces — soft crackles, translucent layers, and subtle shifts of color that bring depth and light to ceramic work.
The series features six distinctive glazes, each reflecting a different aspect of winter’s palette:

KI-11 Snow Drift
a cool, matte white with fine crackles, reminiscent of freshly fallen snow
KI-18 Arctic Blush
a pale rose-pink glaze with frosted undertones, soft and luminous.


KI-21 Winter Glass
a clear blue-aqua glaze with faint veining, suggesting frozen glass.
KI-27 Glacial Lake
a vivid blue-green tone, deep and tranquil like a mountain lake under ice.


KI-46 Frozen Fern
a soft celadon green with delicate crystalline patterns, similar to frost tracing across leaves.
KI-68 Honey Crystal
a warm golden amber glaze that develops gentle crackle highlights.

Each glaze develops unique surface effects depending on clay body, glaze thickness, and firing schedule. While food-safe, the Kiln Ice line is best suited for decorative work due to its fine crackle finish.
The KI Series continues AMACO’s tradition of combining technical refinement with natural beauty – a modern interpretation of classic “ice” and “snowflake” glazes.
How to Use Kiln Ice Glazes – Tips
| Aspect | Recommendation |
|---|---|
| Application | Apply thickly — multiple coats with a soft brush for full “ice crackle” development. |
| Number of coats | Usually 3–4 heavy coats give the strongest crackle. |
| Clay body | Works best on light buff or tan clay bodies without manganese (dark bodies can dull the effect). |
| Underlayers | For dramatic cracks, apply over a dark slip or glaze, e.g. chocolate or black base. |
| Compatibility | Pairs best with glossy or flowing glazes; avoid pairing with stiff matte glazes. |
| Firing | Fire to Cone 5–6 (2167–2232°F / 1186–1222°C). A slow cool cycle can enhance the crackle. |
⚠️ Common Issues
- Weak crackle effect → the glaze layer is too thin or under-fired.
- Too strong / large cracks → over-application or incompatible clay body (COE mismatch).
- Plain crazing without “icy depth” → normal glaze stress; try firing slightly hotter or apply thicker.
- Hairline cracks visible only after cooling → normal for this glaze — they develop during the cool-down.
- Moisture retention → don’t use for food surfaces.
🔍 Quick Troubleshooting
| Symptom | Likely Cause | Fix |
|---|---|---|
| No crackles visible | Glaze too thin | Apply thicker or refire slightly hotter |
| Cracks too wide | Glaze too thick / incompatible clay | Use thinner coats or test on a different clay |
| Milky haze overall | Too thick or over-fired | Thin application or lower cone slightly |
| Bare patches | Uneven coat | Mix glaze thoroughly and brush evenly |
🔬 Technical Notes
- These glazes rely on a mismatch in thermal expansion between glaze and clay to form surface cracks.
- When the piece cools, the glaze contracts faster than the clay body, producing the “ice fracture” effect.
- Each crack catches light differently — that’s why they appear icy and multi-layered.
Here you can find some examples of Kiln Ice