Almost the desired effect…. Will use white clay next time. This was reclaim and it seems to have a large bits of grog that have come to the surface. Not there at bisque 🤔 Fired to 1225 degrees Celsius with 5 min hold
- Clay: reclaim with grog
- Iron Lustre x2
- Purple Crystall x2
- Fired to 1225 C with 5 min hold
Credit:Kay Chandler